From: Laboratory experiments on the effects of corrosion inhibitor on the mechanical properties of reservoir rock

Fig. 7

Microstructures of samples deformed at 20Ā MPa confining pressure, all obtained with under cross-polarized light. a BS-09, Bentheim sandstone deformed with water. b TM4-2, Treuchtlinger Marmor limestone deformed in the presence of water. Gouge-filled localized shear-zone with boundary shear zones, about 100Ā Āµm wide. c TM2-2, Treuchtlinger Marmor limestone deformed in the presence of inhibitor 1 (3000Ā ppm). Incohesive sample, visible, intact, islands in main shear zones, seperated by highly localized fractures, and minimal gouge development. d TM2-3, Treuchtlinger Marmor limestone deformed in the presence of inhibitor 2 (3000Ā ppm). e TM2-3 shown at a greater magnification to show the fracture and damage zone